High-temperature leaching of Middle Timan bauxites together with intermediate products of the sintering stage in the Bayer-sintering process
Chaykin, Leonid Ivanovich, 2015, Candidate of Sciences dissertation
Ural Federal University named after the First President of Russia B.N. Yeltsin, Yekaterinburg
115 pp.
More works in this specialty
- Improvement of the technology for producing pipe steel with low hydrogen content in oxygen-converter shops
Nikolaev, Aleksei Olegovich · Candidate of Sciences · Nosov Magnitogorsk State Technical University
- Increasing the efficiency of metal stirring in the bath by improving the design of a small-capacity direct-current arc furnace
Portnova, Irina Vasil'evna · Candidate of Sciences · South Ural State University
- Improvement of continuous steel casting in order to reduce defects caused by distortion of the slab profile
Shevchenko, Yevgeniy Aleksandrovich · 2015 · Candidate of Sciences · Nosov Magnitogorsk State Technical University
- Improvement of calcination processes for carbon materials based on mathematical modeling
Chibashvili, Alevtina Viktorovna · 2015 · Candidate of Sciences · North Caucasus Mining and Metallurgical Institute
- New components of welding materials using raw materials of the Kola Peninsula: conditioning, synthesis, and interaction
Chekanova, Yuliya Viktorovna · 2015 · Candidate of Sciences · I.V. Tananaev Institute of Chemistry and Technology of Rare Elements and Mineral Raw Materials of the Kola Science Center of the Russian Academy of Sciences